๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

High speed impact on Zr41Ti14Cu12.5Ni10Be22.5 bulk metallic glass

โœ Scribed by C. Yang; R.P. Liu; Z.J. Zhan; L.L. Sun; W.K. Wang


Publisher
Elsevier Science
Year
2006
Tongue
English
Weight
796 KB
Volume
426
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Micro-forming and surface evaluation of
โœ Myoung-Ryul Ok; Jin-Yoo Suh; Sung Jae Chung; Young Su Ji; Kyung Tae Hong ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 828 KB

Bulk metallic glasses are adequate for micro-forming because of the viscous flow in the supercooled liquid state. The deformation behavior of Zr 41 Ti 14 Cu 12.5 Ni 10 Be 22.5 alloy under compression in the supercooled liquid state were investigated by using DSC and TMA. Based on the deformation beh

Characterization of multiple crystalliza
โœ Hyun-Joon Jun; Kwang Seok Lee; Young Won Chang ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 965 KB

The effects of crystallization on the thermal and mechanical properties of Zr 41.2 Ti 13.8 Cu 12.5 Ni 10 Be 22.5 (number indicate at.%) bulk metallic glass (BMG) have been systematically studied by varying annealing times at 400 โ€ข C. An icosahedral quasicrystalline phase was identified in the specim

Corrosion behavior of Zr41.2Ti13.8Ni10Cu
โœ M. Hemmati Pourgashti; E. Marzbanrad; E. Ahmadi ๐Ÿ“‚ Article ๐Ÿ“… 2010 ๐Ÿ› Elsevier Science โš– 457 KB

In this study electrochemical corrosion behavior of Zr 41.2 Ti 13.8 Ni 10 Cu 12.5 Be 22.5 bulk metallic glass (BMG) in various aqueous solutions (3.5% NaCl, 1 N HNO 3 , H 2 SO 4 and HCl) in order to compare with 316L stainless steel were thoroughly investigated. Scanning electron microscopy (SEM) wa

Relaxation and crystallization of Zr41.2
โœ Rex C.Y Tam; C.H Shek ๐Ÿ“‚ Article ๐Ÿ“… 2004 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 260 KB

The influences of relaxation on glass transition and on the crystallization behavior of Zr 41.2 Ti 13.8 Cu 12.5 Ni 10 Be 22.5 bulk amorphous alloys were investigated. The alloys were annealed at 643 K, which was below the glass transition temperature, for different annealing times to investigate the