𝔖 Bobbio Scriptorium
✦   LIBER   ✦

High-pressure and high-temperature differential scanning calorimeter for combined pressure-concentration-temperature measurements of hydrides

✍ Scribed by Mauron, Ph.; Bielmann, M.; Bissig, V.; Remhof, A.; Züttel, A.


Book ID
120401973
Publisher
American Institute of Physics
Year
2009
Tongue
English
Weight
900 KB
Volume
80
Category
Article
ISSN
0034-6748