The photoacoustic signal strength was measured on a series of similar portland cement pastes dried to different water contents. Under appropriate conditions this signal is a function of only the paste's specific heat capacity and thermal conductivity. Because of this, inferences can be made about th
Glassy dynamics of water in hydrated cement paste
โ Scribed by P. Baglioni; E. Fratini; S.-H. Chen
- Book ID
- 106024379
- Publisher
- Springer
- Year
- 2002
- Tongue
- English
- Weight
- 870 KB
- Volume
- 74
- Category
- Article
- ISSN
- 1432-0630
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Samples of hydrating Type I portland cement paste were soaked in a saturated St(OH)2 solution at 80ยฐC for periods from 7 to 28 days. This treatment generates a new and, as yet, unidentified material. The new material has a charaotemistie X-ray pattern, contains ,strontium, and is less porous and m
Data from small-angle X-ray scattering experiments are used to determine the fractal types and dimensions of hydrated portland cement pastes over a range of length scales. The larger-scale, 200-1500 A, geometry at most degrees of water saturation is found to be that of a rough surface fractal. The s