𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Glass Transition of Soy Globulins Using Differential Scanning Calorimetry and Mechanical Spectrometry

✍ Scribed by Alfredo Morales; Jozef L. Kokini


Book ID
109387988
Publisher
American Institute of Chemical Engineers
Year
1997
Tongue
English
Weight
141 KB
Volume
13
Category
Article
ISSN
8756-7938

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Glass transition temperatures of hydroca
✍ Adam S. Cantor πŸ“‚ Article πŸ“… 2000 πŸ› John Wiley and Sons 🌐 English βš– 153 KB πŸ‘ 2 views

A comparison of calculated and measured glass transition temperatures of a series of three-component hydrocarbon blends was performed. The blends were prepared as mixtures of an elastomer with different proportions of tackifying resin and oil. Glass transition temperature, T g , was measured by diff