Gauge length effect on the tensile properties of leather
β Scribed by Palanisamy Thanikaivelan; Dennis C. Shelly; Seshadri S. Ramkumar
- Publisher
- John Wiley and Sons
- Year
- 2006
- Tongue
- English
- Weight
- 291 KB
- Volume
- 101
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
β¦ Synopsis
Abstract
Tensile properties are important basic characteristics of materials and influence their endβuse and performance. More importantly, in the case of leather due to endβuse applications such as shoe uppers, automotive and furniture upholstery, mechanical properties such as tenacity are of extreme importance. Therefore, fundamental studies on the tensile properties of leather are needed. In this study, an attempt has been made to examine the effect of gauge length (GL) on the tensile properties of shoe upper leather. Two different specimens in the form of rectangular and dumbbell shapes have been cut from parallel and perpendicular directions to the body axis of the leather and have been tested. Results showed that the maximum breaking load and the percentage extension at break decreased with the increase in GL. Rectangular specimens showed a 30% decrease in maximum breaking load and a 13% decrease in percentage extension at break, while dumbbell specimens showed reductions in the order of 28 and 6%, respectively, as the GL increased from 9.53 cm to 23.5 cm. Highly varying supramolecular architecture of the collagen matrix and the frictional slippage caused by the free ends present in the collagen fibrils, which induce a weakβlink effect similar to the one found in cotton fibers and yarns, are considered to be the probable reasons for this behavior. A limited scanning electron microscopic study has been undertaken to pictorially represent the breakage of leather at different GLs. Β© 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 1202β1209, 2006
π SIMILAR VOLUMES
Tensile tests were made on polypropylene films as a function of aging temperature from 80 to 130ΠC at a strain rate of 5 cm min 01 . Polypropylene films aged at 60 and 100ΠC and at time intervals up to 180 min were also stretched at the same strain rate. The yield stress and initial modulus were fou