Galvanic corrosion of silver-brass interface of a capacitor
โ Scribed by S. V. S. Narayana Murty; P. Ramesh Narayanan; A. Natarajan
- Book ID
- 104854482
- Publisher
- Springer
- Year
- 1996
- Tongue
- English
- Weight
- 709 KB
- Volume
- 15
- Category
- Article
- ISSN
- 0261-8028
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
## Abstract The carbamate turns out to be a good inhibitor of the corrosion of brass (80/20 and 59/41) in 0.5 N sodium chloride, 1.0 n sodium hydroxide and buffer solutions (NaOH and citric acid, pH 4.4โ6.0). The inhibiting effect depends on inhibitor concentration, so that in some cases corrosion
## Abstract The corrosion of Brass in nitric acid solutions is studied using thermometric, mass loss and polarization methods. The three methods gave almost similar results. The rate of corrosion was found to increase steadily with nitric acid concentration till about 9M where it starts to slow dow