## Abstract In orthodontics, a combination of metallic alloys is placed into the oral cavity during medical treatment and thus the corrosion resistance and ionic release of these appliances is of vital importance. The aim of this study is to investigate the elemental composition, microstructure, ha
β¦ LIBER β¦
Galvanic corrosion between various combinations of orthodontic brackets and archwires
β Scribed by Arash Bakhtari; Thomas Gerard Bradley; William K. Lobb; David W. Berzins
- Book ID
- 113426063
- Publisher
- Elsevier Science
- Year
- 2011
- Tongue
- English
- Weight
- 449 KB
- Volume
- 140
- Category
- Article
- ISSN
- 1097-6752
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Metallurgical characterization, galvanic
β
Myrsini S. Darabara; Lefteris I. Bourithis; Spiros Zinelis; George D. Papadimitr
π
Article
π
2007
π
John Wiley and Sons
π
English
β 487 KB
Evaluation of friction of conventional a
β
Vittorio Cacciafesta; Maria Francesca Sfondrini; Andrea Scribante; Catherine Kle
π
Article
π
2003
π
Elsevier Science
π
English
β 262 KB
Evaluation of friction of stainless stee
β
Vittorio Cacciafesta; Maria Francesca Sfondrini; Andrea Ricciardi; Andrea Scriba
π
Article
π
2003
π
Elsevier Science
π
English
β 236 KB
Reduction of sliding friction between an
β
Chung F. Liew
π
Article
π
1994
π
Elsevier Science
π
English
β 116 KB
Surface characterizations and corrosion
β
Her-Hsiung Huang
π
Article
π
2005
π
John Wiley and Sons
π
English
β 476 KB
## Abstract This study investigated the surface characterizations and corrosion resistance of asβreceived commercial nickelβtitanium (NiTi) dental orthodontic archwires from different manufacturers using a cyclic potentiodynamic test in artificial saliva with various acidities. An atomic force micr
Comparison of frictional forces during t
β
Tae-Kyung Kim; Ki-Dal Kim; Seung-Hak Baek
π
Article
π
2008
π
Elsevier Science
π
English
β 662 KB