Galvanic corrosion behaviour of aluminium 3004 and copper in tropical marine atmosphere

✍ Scribed by Subramanian, G.; Palraj, S.; Palanichamy, S.


Book ID
125375279
Publisher
Harbin Engineering University
Year
2014
Tongue
English
Weight
312 KB
Volume
13
Category
Article
ISSN
1671-9433

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Atmospheric corrosion of galvanized stee
✍ A. I. Almarshad; S. Syed πŸ“‚ Article πŸ“… 2008 πŸ› John Wiley and Sons 🌐 German βš– 122 KB

## Abstract Three‐year exposure programme was carried out in Saudi Arabia at nine test stations with different climatic and pollution conditions. The aim of this study was to evaluate the joint effect of atmospheric pollutants (Cl^βˆ’^ and SO~2~), relative humidity (RH) and temperature (T) on the atm