✦ Synopsis
This paper presents a three-dimension radiograph detector for inspecting the location of weld defects and their sizes, including spilly place, aircavity, slag inclusion, uncomplete weld of edge joint. Confirmed by the actual dissection of weld, the testing results show that the absolute error is less than 0.3 mm and the relative error less than 5%.
📜 SIMILAR VOLUMES
This paper presents a three-dimension radiograph detector for inspecting the location of weld defects and their sizes, including spilly place, aircavity, slag inclusion, uncomplete weld of edge joint. Confirmed by the actual dissection of weld, the testing results show that the absolute error is les