Polypropyleneโwood fiber composites: Eff
โ
Fernanda M.B. Coutinho; Thais H.S. Costa; Daisy L. Carvalho
๐
Article
๐
1997
๐
John Wiley and Sons
๐
English
โ 246 KB
๐ 2 views
Polypropylene/wood fiber composites were prepared at three different temperatures: 170ะC, 180ะC, and 190ะC. The surface of wood fibers was modified through the use of silane coupling agents and/or coating with polypropylene or maleated polypropylene. The fiber coating was performed by propylene poly