Sintering temperature, ranging between 350 and 2700Β°C was studied to discern its influence on the characteristics of carbons made from mesocarbon microbeads (MCMB) of size 4-16 m. These were formed in a coal tar pitch by heat treatment at 420Β°C for 2.5 h, and separated by solvent extraction using a