Fracture toughness and fractography of cast and extruded 7075 AlSiC particulate composites

✍ Scribed by Kulkarni, M.D.; Robi, P.S.; Prasad, R.C.; Ramakrishnan, P.


Book ID
122544350
Publisher
Elsevier Science
Year
1994
Weight
481 KB
Volume
31
Category
Article
ISSN
0956-716X

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Mechanical properties and fractography o
✍ S.C Sharma; K.H.W Seah; B.M Girish; R Kamath; B.M Satish 📂 Article 📅 1997 🏛 Elsevier Science ⚖ 363 KB

This paper reports an investigation of the mechanical properties of as-cast lead᎐antimony alloy composites containing quartz particles of size 30᎐50 m and of contents ranging from 0 to 12% in steps of 4% by weight. The ' vortex method' was used to produce the composites. The result of the study reve