๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Fracture mechanics approach to the study of stress corrosion cracking of austenitic stainless steel clad metals

โœ Scribed by K. N. Krishnan; K. Prasad Rao


Publisher
Springer
Year
1991
Tongue
English
Weight
945 KB
Volume
10
Category
Article
ISSN
0261-8028

No coin nor oath required. For personal study only.