𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Fractography of ice

✍ Scribed by E. M. Schulson; I. Baker; C. D. Robertson; R. B. Bolon; R. J. Harnimon


Publisher
Springer
Year
1989
Tongue
English
Weight
601 KB
Volume
8
Category
Article
ISSN
0261-8028

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Possibilities of Fractography
✍ M. A. Shtremel' πŸ“‚ Article πŸ“… 2005 πŸ› Springer US 🌐 English βš– 125 KB
Fractals in fractography
✍ Ervin E Underwood; Kingshuk Banerji πŸ“‚ Article πŸ“… 1986 πŸ› Elsevier Science βš– 929 KB
Notch sensitivity and fractography of po
✍ R. D. Goolsby; A. M. Chatterjee πŸ“‚ Article πŸ“… 1983 πŸ› Society for Plastic Engineers 🌐 English βš– 942 KB

## Abstract The notch sensitivity of high‐density polyethylene (HDPE), polypropylene (PP), and polybutylene (PB) was evaluated using uniaxial tensile deformation and fractographic analysis. Each polyolefin was tested at relatively low and high molecular weights (MW). Only the lower MW HDPE was foun