Pulse-electrodeposited nanonickel was heat-treated to produce grain sizes from nanoscale to microscale. The hardness of individual grains was examined by nanoindentation. The results show that hardness not only depends on the grain size, but also on the ratio of grain size to the indent size. Beside
Widely used the Bulychev-Alekhin-Shorshorov relation for analyzing nanoindentation load-displacement data to determine elastic modulus of a thin specimen does not account for the size of specimen since the BASh relation is based on analytical solutions of the contact problems for an elastic half-spa