𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Fatigue life assessment of aluminium alloys with casting defects

✍ Scribed by B. Skallerud; T. Iveland; G. Harkegard


Publisher
Elsevier Science
Year
1994
Tongue
English
Weight
188 KB
Volume
16
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.