Unacceptably high leakage rates from a large number of type 304 stainless steel tubes forced the scrapping of two carbonate reboiler heat exchangers from the carbon dioxide removal system of a fertilizer plant. Extensive failure investigation carried out on the failed heat exchangers established tha
Failure analysis of 101-C ammonia plant heat exchanger
β Scribed by S.A.J. Jahromi; M.M. AliPour; A. Beirami
- Publisher
- Elsevier Science
- Year
- 2003
- Tongue
- English
- Weight
- 1022 KB
- Volume
- 10
- Category
- Article
- ISSN
- 1350-6307
No coin nor oath required. For personal study only.
β¦ Synopsis
Long-term overheating is a major cause of failures in boiler tubes of different designs and operation conditions. These failures are usually related to the formation and growth of internal oxide scales or deposits at areas of high heat flux. Deposits might have different sources; poor water treatment and general corrosion in the system are two common types of these sources. Thickening of the deposit layer hinders heat transfer and local spots of high metal temperature are created in the tube wall. With increasing metal temperature, creep becomes much faster leading to tube failure under internal pressure. In this paper, a case history involving this type of failure is presented. Using finite element modeling the failure are analyzed and some methods to prevent this type of failure are recommended.
π SIMILAR VOLUMES