Dielectric relaxation and giant dielectr
β
Liu, Peng ;He, Ying ;Zhou, Jian-ping ;Mu, Chun-hong ;Zhang, Huai-wu
π
Article
π
2009
π
John Wiley and Sons
π
English
β 582 KB
## Abstract CaCu~3~Ti~4β__x__~ Nb__~x~__ O~12~ (__x__ = 0, 0.01, 0.08, 0.2) ceramics were fabricated by a conventional solidβstate reaction method. The ceramics showed the bodyβcentered cubic structure without any foreign phases and the grain size decreases with Nb doping. Two Debyeβtype relaxation