𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Evaluation of viscoelastic properties of materials by nanoindentation

✍ Scribed by S. O. Abetkovskaia; S. A. Chizhik; V. A. Rudnitsky; A. P. Kren


Book ID
111506685
Publisher
Allerton Press, Inc.
Year
2010
Tongue
English
Weight
247 KB
Volume
31
Category
Article
ISSN
1068-3666

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES