Evaluation of fatigue crack initiation in a notched single-crystal superalloy component

✍ Scribed by Daniel Leidermark; Johan Moverare; Mikael Segersäll; Kjell Simonsson; Sören Sjöström; Sten Johansson


Publisher
Elsevier
Year
2011
Tongue
English
Weight
280 KB
Volume
10
Category
Article
ISSN
1877-7058

No coin nor oath required. For personal study only.

✦ Synopsis


The fatigue crack initiation in a notched single-crystal nickel-base superalloy component at 500°C was investigated and analysed. A critical plane approach in combination with a critical distance method has been adopted, in which the total shear strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to predict the number of cycles to fatigue crack initiation. The experimental test specimens were studied by microscopy to determine on which crystallographic plane the fatigue initiation occurred. A good correlation between the experimental results and the simulated results were found.


📜 SIMILAR VOLUMES


Fatigue life evaluation of a single crys
✍ Motoki Sakaguchi; Masakazu Okazaki 📂 Article 📅 2007 🏛 Elsevier Science 🌐 English ⚖ 333 KB

A new micromechanics model was proposed to estimate the effects of microstructural geometry on fatigue life of single crystal Ni-base superalloys. The Eshelby's theory, the averaging field approximation and the hybrid composite theory were combined and extended so that it makes possible to discuss m