𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Evaluation of Crack Growth in Glass by Using Stress-Wave Fractography

✍ Scribed by Satoshi Yoshida; Jun Matsuoka; Naohiro Soga


Book ID
110827820
Publisher
John Wiley and Sons
Year
2004
Tongue
English
Weight
195 KB
Volume
82
Category
Article
ISSN
0002-7820