Evaluation of a capillary tube sample container for differential scanning calorimetry

✍ Scribed by L.F. Whiting; M.S. Labean; S.S. Eadie


Publisher
Elsevier Science
Year
1988
Tongue
English
Weight
919 KB
Volume
136
Category
Article
ISSN
0040-6031

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Efficiency of antioxidants in thick-wall
✍ B. Stenberg; F. BjΓΆrk πŸ“‚ Article πŸ“… 1986 πŸ› John Wiley and Sons 🌐 English βš– 308 KB πŸ‘ 2 views

The effect ot two antioxidants, IPPD and DENA, on the aging properties of TMTD-vulcanized natural rubber was studied by DSC. In the case of IPPD, the results were compared with mechanical measurements. The DSC measurements were carried out on specimens taken at different depths from cylindrical samp