𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Er+As Ion Implantation to Reduce Stress Corrosion Cracking of Generator Retaining Ring Steel in Nitrate Solution

✍ Scribed by Jin, H.; Kim, H. J.; Woerner, D.; Wu, C. L.


Book ID
120977878
Publisher
NACE International
Year
2002
Tongue
English
Weight
111 KB
Volume
58
Category
Article
ISSN
0010-9312

No coin nor oath required. For personal study only.