Enhancing resistance to pitting corrosion in mechanically polished stainless steel 316 LVM by water treatment

โœ Scribed by P.E. Klages; Z. Bai; M. Lobban; M.K. Rotermund; H.H. Rotermund


Book ID
113595972
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
943 KB
Volume
15
Category
Article
ISSN
1388-2481

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Improvement of pitting corrosion resista
โœ T. Bellezze; G. Roventi; A. Quaranta; R. Fratesi ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 451 KB ๐Ÿ‘ 1 views

## Abstract The pitting corrosion resistance of AISI 444, 304L and 316L stainless steels in two tap waters with different chloride concentrations at 80โ€‰ยฐC was studied. Cyclic potentiodynamic polarization (CPP) tests were carried out starting from __E__~corr~โ€‰โˆ’โ€‰30 mV until the current density reache