✦ LIBER ✦
Electron fractographic investigation of fracture surfaces of Armco iron tested to rupture in uniaxial tension in air and during electrolytic hydrogen charging
✍ Scribed by N. Ya. Yaremchenko; M. M. Shved; G. V. Karpenko
- Publisher
- Springer
- Year
- 1973
- Tongue
- English
- Weight
- 570 KB
- Volume
- 6
- Category
- Article
- ISSN
- 1573-885X