✦ LIBER ✦
Electrochemical and stress corrosion cracking behavior of 67Cu–33Zn alloy in aqueous electrolytes containing chloride and nitrite ions: Effect of di-sodium hydrogen phosphate (DSHP)
✍ Scribed by Nageh K. Allam; Elsayed A. Ashour
- Publisher
- Elsevier Science
- Year
- 2009
- Tongue
- English
- Weight
- 974 KB
- Volume
- 156
- Category
- Article
- ISSN
- 0921-5107
No coin nor oath required. For personal study only.