๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Electrical conductivity of vapor-grown carbon fibers

โœ Scribed by J. Heremans


Publisher
Elsevier Science
Year
1985
Tongue
English
Weight
548 KB
Volume
23
Category
Article
ISSN
0008-6223

No coin nor oath required. For personal study only.

โœฆ Synopsis


Carbon fibers grown by pyrolysis of natural gas were heat-treated at temperatures ranging from 1400 to 3OOO"C, and characterized by X-ray diffraction. Their electrical resistivity is reported for temperatures between 10 and 370 K, and explained for heat treatment above 2200ยฐC using a simple graphitic band model. Filaments heat-treated at lower temperatures and as-grown fibers show a resistivity with a small temperature dependence.


๐Ÿ“œ SIMILAR VOLUMES


Vapor-grown carbon-fiber reinforced carb
โœ Jyh-Ming Ting; Max L. Lake ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 710 KB

Vapor-grown carbon-fiber (VGCF) reinforced carbon (VGCF-C) composites were studied for thermal and physical properties. Effect of fiber volume fraction and final density of composite on thermal conductivity was investigated. The fiber volume fractions range from 25 v/o to 36% and the final densitie

Mechanical properties of vapor-grown car
โœ R.L. Jacobsen; T.M. Tritt; J.R. Guth; A.C. Ehrlich; D.J. Gillespie ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 529 KB

The elastic properties of individual vapor-grown carbon fibers have been studied via the lowstrain, vibrating-reed technique. The average Young's modulus is found to be 680 GPa, with some indication that the intrinsic modulus of CVD carbon may be much higher. This value exceeds those found by earli

Vapor-grown carbon fibers from benzene p
โœ Mahalingam Jayasankar; Ramesh Chand; santosh K. Gupta; D. Kunzru ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 616 KB

Carbon fibers were grown on alumina substrates by vapor phase decomposition of benzene in the presence of hydrogen in a tubular reactor. The effect of lengthening duration and temperature on the average fiber length was studied at two different benzene concentrations (13.2 and 18.6 mol%). In the tem