Effects of viscoelasticity and time-dependent plasticity on nanoindentation measurements of human cortical bone
✍ Scribed by Fan, Zaifeng ;Rho, Jae-Young
- Publisher
- John Wiley and Sons
- Year
- 2003
- Tongue
- English
- Weight
- 163 KB
- Volume
- 67A
- Category
- Article
- ISSN
- 0021-9304
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
The viscoelastic and time‐dependent plastic effects on the nanoindentation measurement of osteonal lamella in a human cortical bone were investigated. The elastic modulus of osteonal lamella obtained from the quasi‐static technique was strongly affected by the indentation rate and time‐dependent plasticity. The effects of time‐dependent plasticity can be diminished by multiple loading–unloading cycles and a long holding period at maximal load. After minimizing the contribution of time‐dependent plasticity to unloading data, it was surprisingly found that the elastic modulus was proportional to indentation strain rate raised to the 0.06 power, which is similar to conventional test results. © 2003 Wiley Periodicals, Inc. J Biomed Mater Res 67A: 208–214, 2003
📜 SIMILAR VOLUMES
## Abstract We have previously shown, using Dynamic Mechanical Analysis (DMA), that the presence of a defect in cortical bone tissue affects the apparent viscoelastic properties of that bone. However, mechanically induced damage is more complex than a machined defect making it difficult to predict
## Abstract The effects of two key experimental parameters on the measured nanomechanical properties of lamellar and interlamellar tissue were examined in dehydrated rabbit cancellous bone. An anhydrous sample preparation protocol was developed to maintain surface integrity and produce RMS surface
## Abstract The viscoelastic properties of cancellous bone can be measured nondestructively in compression testing using a dynamic mechanical analyzer. In this study, we examined the effects of end boundary conditions and specimen geometry on the viscoelastic properties of cancellous bone measured
The effects of water loss on the T 1 and T 2 \* of bovine cortical bone were investigated using ultrashort echo time sequences with signals excited either by a short hard pulse or by two longer half pulses. Nine bovine femur samples were prepared and sequentially air-and oven-dried. On average 3.42%
## Abstract Bioactive glasses dissolve upon immersion in culture medium, and release their constitutive ions into solution. There has been some evidence suggesting that these ionic‐dissolution products influence osteoblast‐specific processes. Here, the effect of 58S sol–gel‐derived bioactive glass