Effects of loading waveform on fatigue crack growth of Udimet 720 Li superalloy

✍ Scribed by G. Onofrio; G.A. Osinkolu; M. Marchionni


Book ID
108401242
Publisher
Elsevier Science
Year
2004
Tongue
English
Weight
420 KB
Volume
26
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


The effects of environment and loading w
✍ M.R Bache; W.J Evans; M.C Hardy 📂 Article 📅 1999 🏛 Elsevier Science 🌐 English ⚖ 950 KB

The influence of environment and fatigue waveform shape on crack growth behaviour has been evaluated in a workhorse turbine disc material, Inconel 718, at 600°C through an experimental programme that investigated crack growth from a notch geometry. Crack growth data are presented for a variety of st

Effects of Loading Waveform and Stress F
✍ P. Heuler; E. Affeldt; R.J.H. Wanhill 📂 Article 📅 2003 🏛 John Wiley and Sons 🌐 English ⚖ 325 KB

## Abstract High temperature fatigue in nickel‐base superalloys for aero‐engine applications requires consideration of cycle‐ and time‐dependent phenomena. For waveforms with dwells and/or low frequencies crack growth rates may be significantly accelerated up to the point of fully time‐dependent cr