Effects of heat treatment and HIP on creep properties of Ni-base superalloy IN713LC: Y.S. Kim, et al, (Chosan University, Kwang Ju, Korea), J. Korean Inst. of Metals, Vol 28, No 10, 1990, 866–872. In Korean