The effects of chromium addition and hea
✍
P.I. Ferreira; A.A. Couto; J.C.C. de Paola
📂
Article
📅
1995
🏛
Elsevier Science
🌐
English
⚖ 531 KB
Fe-24Al (at.%) base alloys containing O-6 at.% Cr were elaborated by melting and casting under argon atmosphere. The ingots obtained were initially homogenized at 1000 "C for 5 h in air, then hot rolled at temperatures in the range 1000-800 "C. The hot rolled strips obtained were submitted to two he