Al 2 O 3 , SiC and kaolin were employed as additives in combustion synthesizing Al 2 O 3 -TiB 2 ceramic composite. Effects of the additives on adiabatic temperature, combustion wave velocity, volume change and composite density were studied, and bending strength of the synthesized ceramics was evaluated. By theoretical calculation, the adiabatic temperature of Al-TiO 2 -H 3 BO 3 system is 2314.85 • C and decreases with increasing the additive addition. With Al 2 O 3 addition, the phases presented in the ceramic composite are unchanged, and the phases of SiC and 3Al 2 O 3 •2SiO 2 emerges when SiC and kaolin are added. The addition of the additives results in a refined TiB 2 particulate size and reduces combustion wave velocity. The highest density is achieved with the addition of kaolin from 10 to 30 wt.% making the volume change from -4.6 to -1.2%. The bending strength of the TiB 2 -Al 2 O 3 composite is improved eight times with the addition of 30 wt.% kaolin.


📜 SIMILAR VOLUMES


Sintering and characterization of Al2O3-
✍ Isao Kimura; Noriyasu Hotta; Yukio Hiraoka; Natsukaze Saito; Yuji Yokota 📂 Article 📅 1989 🏛 Elsevier Science 🌐 English ⚖ 476 KB

## A bstra ct AI203-TiB 2 composites containing 0-50 wt% TiB 2 were prepared by sintering at 1600-1750°C ,for 15-120min in a vacuum. Relative density increased with TiB 2 addition from 97% (no TiB2) to about 99% ( lO-40wt% TiB2) on sintering at 1750°C Jbr 60 min. TiB 2 behaved as a sintering aid t