The coefficient of thermal expansion (CTE) and accumulated plastic strain of the pure aluminum matrix composite containing 50% SiC particles (Al/SiC p ) during thermal cycling (within temperature range 298-573 K) were investigated. The composite was produced by infiltrating liquid aluminum into a pr
## Abstract Stem modularity in total hip replacement introduces an additional taper joint between Tiβ6Alβ4V stem components with the potential for fretting corrosion processes. One possible way to reduce the susceptibility of the Tiβ6Alβ4V/Tiβ6Alβ4V interface to fretting is the surface modification