The low melting point of Sn-In alloys opens them a broad field of industrial applications, especially as Pb free solders. Sn-9.8 wt% In alloy is investigated for its structure and creep behaviour. The X-ray diffraction analysis shows that the slowly cooled sample contains both the b-Sn phase and the
Effect of Temperature and Stress on the Structure and Creep Parameters of Pb—2 at% Sb Alloy
✍ Scribed by Al-Ganainy, G. S. ;Mostafa, M. T. ;Nagy, M. R. ;Al-Ganainy, G. S.
- Publisher
- John Wiley and Sons
- Year
- 1998
- Tongue
- English
- Weight
- 236 KB
- Volume
- 165
- Category
- Article
- ISSN
- 0031-8965
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract The work examines the structural transitions of DNA under the action of Cu^2+^ and Ca^2+^ ions in aqueous solution at temperatures of 29 and 45°C by ir spectroscopy. Upon binding to the divalent ions studied, DNA transits into the compact state both at 29 and 45°C. In the compact state
Large unilamellar dipalmitoylphosphatidylcholine (DPPC) and dipalmitoylphosphatidylglycerol (DPPG) liposomes loaded with an aqueous chemotherapeutic drug, cytosine arabinofuranoside (ARA-C), were exposed for 30 min to 60 W/kg continuous-wave (CW) 100-MHz or 2.45-GHz radiation in vitro at temperature