Effect of solution treatment on the hot workability of electroslag remelted Ni−Cr−Mo alloy
✍ Scribed by Tae-Kyu Kim; Jinsung Jang; Jun-Hwa Hong
- Publisher
- TechnoPress
- Year
- 2002
- Tongue
- English
- Weight
- 1017 KB
- Volume
- 8
- Category
- Article
- ISSN
- 1598-9623
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Hot-torsion tests have been carried out at 310 and 370 °C (at a strain rate of l s-i) on an AA 2024 aluminium alloy homogenized for 8 h at between 420 and 520 °C and either just water quenched or air cooled and aged at 290 or 350 °C. The flow curves exhibited a large peak stress ap and work softenin
## Abstract The objective of this investigation was to study the compositional influence on the corrosion behavior of Ni‐Cr‐Mo dental casting alloys in acidic artificial saliva. Cyclic potentiodynamic and potentiostatic tests were used to evaluate the corrosion behavior of different Ni‐Cr‐Mo dental