𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Effect of solidification conditions on MC carbides in a nickel-base superalloy IN 738 LC

✍ Scribed by Liu, L.; Sommer, F.; Fu, H.Z.


Book ID
122345098
Publisher
Elsevier Science
Year
1994
Weight
358 KB
Volume
30
Category
Article
ISSN
0956-716X