๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Effect of Porosity on the Capacity Fade of a Lithium-Ion Battery

โœ Scribed by Sikha, Godfrey; Popov, Branko N.; White, Ralph E.


Book ID
118125326
Publisher
The Electrochemical Society
Year
2004
Tongue
English
Weight
247 KB
Volume
151
Category
Article
ISSN
0013-4651

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES