Effect of particle size on the creep rate of superalloy Inconel 718

โœ Scribed by M.C. Chaturvedi; Y. Han


Publisher
Elsevier Science
Year
1987
Weight
315 KB
Volume
89
Category
Article
ISSN
0025-5416

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Effect of Particle Size on Rate of Coale
โœ Sheryl H. Ehrman ๐Ÿ“‚ Article ๐Ÿ“… 1999 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 51 KB

In high temperature processes, at high concentrations, aerosol particles grow by collisions and coalescence. The rate of coalescence is an important parameter for predicting the final primary particle size. For some materials, particularly silica, predictions of final primary particle size using coa

Surface Roughness and Particle Size Effe
โœ S.Yu. Shulepov; G. Frens ๐Ÿ“‚ Article ๐Ÿ“… 1996 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 144 KB

11), hydrophobic interaction (12, 13), secondary minimum The influence of particle size on the kinetics of slow Brownian coagulation (6-8, 14-16), slow equilibration of the surface coagulation is studied. Colloidal gold was chosen as a model syscharge during the collisions (17, 18), etc.-into tradit

Effect of Particle Size on the Sticking
โœ Rene C. van Duijvenbode; Ger J.M. Koper ๐Ÿ“‚ Article ๐Ÿ“… 2001 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 44 KB

In the literature the transport of particles toward an oppositely charged collector in stagnation point flow is described theoretically with the Smoluchowski-Levich solution of the convective-diffusion equation. Using optical reflectometry, the initial adsorption rate in the case of adsorption of ne