๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Effect of machining operations on the stress-corrosion cracking of steel 40Kh

โœ Scribed by Yu. I. Babei; I. I. Vasilenko; I. V. Karpenko


Publisher
Springer
Year
1967
Tongue
English
Weight
991 KB
Volume
2
Category
Article
ISSN
1573-885X