Effect of heat treatment on pitting corrosion resistance of 6061 Al/SiCPcomposite coated by the cerium oxide film in 3.5 N NaCl solution
✍ Scribed by S. Rajasekaran; N. K. Udayashankar; Jagannath Nayak