The use of plant fibers as a reinforcement in polyester matrices requires the issue of compatibility between the two phases to be addressed. Because plant fibers present hydrophilic surfaces and polyesters are generally hydrophobic, poor fibermatrix dispersion and wetting of the fibers by the matrix may result. As a consequence, the mechanical properties of the composite are severely reduced. This study considers the effect of fiber treatment by chemical modification of the fibers (acetylation) or the use of silane or titanate coupling agents on the mechanical properties of coir or oil palm reinforced polyester composites.
π SIMILAR VOLUMES
Pineapple leaf fiber (PALF) which is rich in cellulose, relatively inexpensive, and abundantly available has the potential for polymer reinforcement. The present study investigated the tensile, flexural, and impact behavior of PALF-reinforced polyester composites as a function of fiber loading, fibe
The partial impregnation textile preform consisting of chopped-strand, long glass fiber and nonwoven polypropylene (PP) has been prepared by needle-punching to improve fiber-matrix distribution before processing. These unconsolidated textile preforms were then preheated and hot-pressed for consolida
The degree of mechanical reinforcement that could be obtained by the introduction of henequen cellulosic fibers in a low-density polyethylene, LDPE, matrix was assessed experimentally. Composite materials of LDPE-henequen cellulosic fibers were prepared by mechanical mixing. The concentration of ran
The thermal conductivity and thermal diffusivity of oil-palm-fiber-reinforced untreated (Sample 1) and differently treated composites were measured with the transient plane source technique at room temperature and under normal pressure. All the composites were 40% oil-palm fiber by weight. The fiber
Polypropylene/wood fiber composites were prepared at three different temperatures: 170ΠC, 180ΠC, and 190ΠC. The surface of wood fibers was modified through the use of silane coupling agents and/or coating with polypropylene or maleated polypropylene. The fiber coating was performed by propylene poly