𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Effect of BTA on electrochemical corrosion and stress corrosion cracking behaviour of type 304 stainless steel in 1 M HCl

✍ Scribed by A. Devasenapathi; V. S. Raja


Book ID
110320797
Publisher
Springer
Year
1998
Tongue
English
Weight
515 KB
Volume
33
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.