𝔖 Bobbio Scriptorium
✦   LIBER   ✦

DNA Functionalization of Carbon Nanotubes for Ultrathin Atomic Layer Deposition of High κ Dielectrics for Nanotube Transistors with 60 mV/Decade Switching

✍ Scribed by Lu, Yuerui; Bangsaruntip, Sarunya; Wang, Xinran; Zhang, Li; Nishi, Yoshio; Dai, Hongjie


Book ID
127373088
Publisher
American Chemical Society
Year
2006
Tongue
English
Weight
241 KB
Volume
128
Category
Article
ISSN
0002-7863