Dissimilar autogenous full penetration welding of superalloy K418 and 42CrMo steel by a high power CW Nd:YAG laser
✍ Scribed by Xiu-Bo Liu; Gang Yu; Ming Pang; Ji-Wei Fan; Heng-Hai Wang; Cai-Yun Zheng