## Abstract Dislocations in the spinodal alloy Fe~30~Ni~20~Mn~25~Al~25~, which is composed of alternating BCC and B2 (ordered BCC) phases, have been investigated using weak‐beam transmission electron microscopy (TEM). The alloy was compressed at room temperature in an as‐hot‐extruded state to strai
7he microstructure and mechanical properties of an austenitic . %C alloy after aging in the temperature range between 743 and 873 K have been investigated. The occurrence of spinodal decomposition was confirmed by transmission electron microscopy observation of a modulated structure with superlattic
In the present study, an Fe-28Mn-6Si-5Cr-0.53Nb-0.06C (mass%) alloy was employed to investigate the influence of laser beam welding (LBW), electron beam welding (EBW) and tungsten-insert gas welding (TIGW) on shape memory properties. This alloy was recently found to exhibit very good shape memory ef