๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Differential scanning calorimetry study of constrained groove pressed low carbon steel: recovery, recrystallisation and ferrite to austenite phase transformation

โœ Scribed by Khodabakhshi, F.; Kazeminezhad, M.


Book ID
126307361
Publisher
Institute of Materials, Minerals and Mining
Year
2013
Tongue
English
Weight
412 KB
Volume
30
Category
Article
ISSN
0267-0836

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES