Phase transitions in a two-dimensional m
โ
Maris, Thierry; Chanh, Nguyen Ba; Bissey, Jean-Claude; Filloleau, Nathalie; Flan
๐
Article
๐
1998
๐
Taylor and Francis Group
๐
English
โ 753 KB