Differential scanning calorimetry studies of the cure of carbon fiber–epoxy composite prepregs

✍ Scribed by Roger J. Morgan; Connie M. Walkup; Tom H. Hoheisel


Publisher
John Wiley and Sons
Year
1985
Tongue
English
Weight
460 KB
Volume
30
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Kinetics of aryl phosphinate anhydride c
✍ Chen, Leo-Wang; Fu, Shih-Chi; Cho, Ching-Sheng 📂 Article 📅 1998 🏛 John Wiley and Sons 🌐 English ⚖ 265 KB 👁 2 views

The curing reaction of two kinds of epoxy resins, (bisphenol A epoxy DER331, and novolac epoxy DEN438) with aryl phosphinate anhydride (9,10dihydro-9-oxa-10-phosphaphenanthrene-10-oxide)-methyl succinic anhydride (DMSA), and benzyldimethylamine (BDMA) as the catalyst, was investigated by di †erentia