𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Differential scanning calorimetry studies and corrosion behavior of the copper clustering stage of Fe73.5−XCu1Nb3Si13.5B9CrX(0,4) amorphous alloys

✍ Scribed by F.F Marzo; A.R Pierna


Book ID
116667366
Publisher
Elsevier Science
Year
2003
Tongue
English
Weight
315 KB
Volume
329
Category
Article
ISSN
0022-3093

No coin nor oath required. For personal study only.