๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Differential scanning calorimetry of spun and drawn polyester yarn

โœ Scribed by S. B. Warner


Book ID
105463809
Publisher
Springer Netherlands
Year
1983
Tongue
English
Weight
250 KB
Volume
28
Category
Article
ISSN
0022-5215